Air Spring
location: Home > Products > Air Spring



Air Spring 2607016
| No. | Property Name | Performance Requirements |
1 | Hardness, Shore A | 60±5 |
| 2 | Tensile Strength, | ≥15 MPa |
| 3 | Elongation at Break, | ≥400 % |
| 4 | After 7 days aging at 70℃ | Hardness change ≤±8 A, Tensile strength change ≤-20%, Elongation at break change ≤-20% |
| 5 | Flex Cracking, Thousands of times | ≥100 |
| 6 | Low Temperature Brittleness | ≤-40℃ |
| 7 | Airtightness Requirement | 24h, Internal pressure drop ≤0.02Mpa |
| 8 | Burst Pressure | ≥3.2Mpa |
| 9 | Fatigue Test | ≥6.5 million times (in good condition) |
| 10 | Neutral Salt Spray Test | ≥200h |

|
No. |
Property Name | Performance Requirements |
| 1 | Hardness, Shore A | 60±5 |
| 2 | Tensile Strength, MPa | ≥15 |
| 3 | Elongation at Break, % | ≥400 |
| 4 | After 7 days aging at 70℃ | Hardness change ≤±8 A, Tensile strength change ≤-20%, Elongation at break change ≤-20% |
| 5 | Ozone Resistance (120h, 100pphm, 40℃, 20% elongation) | No cracking |
| 6 | Flex Cracking, Thousands of times | ≥100 |
| 7 | Low Temperature Brittleness | ≤-40℃ |
| 8 | Airtightness Requirement | 24h, Internal pressure drop ≤0.02Mpa |
| 9 | Burst Pressure | ≥3.2Mpa |
| 10 | Fatigue Test | ≥6.5 million times (in good condition) |
| 11 | Neutral Salt Spray Test | ≥200h |